Porous-surfaced Ti implant compacts, with a solid core surrounded by a porous layer, were self-assembled byelectro-discharge-sintering directly from spherical Ti powders. During an electro-discharge, instant high temperaturesthrough the Ti powder column ranged from 1093 to 4925 °C were generated in times as short as86-153 μsec. At the same time, pinch pressures ranging from 11 to 38 MPa were applied, especially to the middleof the Ti powder column. The solid core size depended on both the pinch pressure magnitude and theheat generated during a discharge. Both the pinch pressure (to squeeze and deform Ti powder particles), and theheat (to weld them together), were key factors in the production of porous-surfaced Ti implant compacts. It isthus suggested that the input energy at constant capacitance is a controllable electro-discharge parameteraffecting the porosity and strength of the porous-surfaced Ti implant compacts.

목차

등록된 정보가 없습니다.

참고문헌 (33)

참고문헌 신청

함께 읽어보면 좋을 논문

논문 유사도에 따라 DBpia 가 추천하는 논문입니다. 함께 보면 좋을 연관 논문을 확인해보세요!

이 논문의 저자 정보

최근 본 자료

전체보기

댓글(0)

0