메뉴 건너뛰기
.. 내서재 .. 알림
소속 기관/학교 인증
인증하면 논문, 학술자료 등을  무료로 열람할 수 있어요.
한국대학교, 누리자동차, 시립도서관 등 나의 기관을 확인해보세요
(국내 대학 90% 이상 구독 중)
로그인 회원가입 고객센터 ENG
주제분류

추천
검색
질문

논문 기본 정보

자료유형
학술저널
저자정보
Weon-Gu Lee (DS Mirae-tech) Kyoung-Hee Gu (Pukyong National University) Cheol-Su Kim (Pukyong National University) Ki-Woo Nam (Pukyong National University)
저널정보
한국해양공학회 한국해양공학회지 한국해양공학회지 제35권 제5호(통권 제162호)
발행연도
2021.10
수록면
327 - 335 (9page)

이용수

표지
📌
연구주제
📖
연구배경
🔬
연구방법
🏆
연구결과
AI에게 요청하기
추천
검색
질문

초록· 키워드

오류제보하기
Microcracks can rapidly grow and develop in high-strength steels used in offshore structures. It is important to render these microcracks harmless to ensure the safety and reliability of offshore structures. Here, the dependence of the aspect ratio (As) of the maximum depth of harmless crack (α<SUB>hlm</SUB>) was evaluated under three different conditions considering the threshold stress intensity factor (△K<SUB>th</SUB>) and residual stress of offshore structural steel F690. The threshold stress intensity factor and fatigue limit of fatigue crack propagation, dependent on crack dimensions, were evaluated using Ando"s equation, which considers the plastic behavior of fatigue and the stress ratio. α<SUB>hlm</SUB> by peening was analyzed using the relationship between △K<SUB>th</SUB> obtained by Ando"s equation and △K<SUB>th</SUB> obtained by the sum of applied stress and residual stress. The plate specimen had a width 2W = 12 mm and thickness t = 20 mm, and four value of As were considered: 1.0, 0.6, 0.3, and 0.1. The α<SUB>hlm</SUB> was larger as the compressive residual stress distribution increased. Additionally, an increase in the values of As and △K<SUB>th(l)</SUB> led to a larger α<SUB>hlm</SUB>. With a safety factor (N ) of 2.0, the long-term safety and reliability of structures constructed using F690 can be secured with needle peening. It is necessary to apply a more sensitive non-destructive inspection technique as a non-destructive inspection method for crack detection could not be used to observe fatigue cracks that reduced the fatigue limit of smooth specimens by 50% in the three types of residual stresses considered. The usefulness of non-destructive inspection and non-damaging techniques was reviewed based on the relationship between α<SUB>hlm</SUB> , α<SUB>NDI</SUB> (minimum crack depth detectable in non-destructive inspection), α<SUB>crN</SUB> (crack depth that reduces the fatigue limit to 1/N ), and As.

목차

ABSTRACT
1. Introduction
2. Materials and Experimental Methods
3. Results and Discussion
4. Conclusion
References

참고문헌 (28)

참고문헌 신청