메뉴 건너뛰기
.. 내서재 .. 알림
소속 기관/학교 인증
인증하면 논문, 학술자료 등을  무료로 열람할 수 있어요.
한국대학교, 누리자동차, 시립도서관 등 나의 기관을 확인해보세요
(국내 대학 90% 이상 구독 중)
로그인 회원가입 고객센터 ENG
주제분류

추천
검색

논문 기본 정보

자료유형
학술저널
저자정보
Javed S. Ibrahim (Indian Institute of Technology Bombay) M. J. N. V. Prasad (Indian Institute of Technology Bombay) Partha Sarkar (Theis Precision Steel India Private Limited) K. Narasimhan (Indian Institute of Technology Bombay)
저널정보
대한금속·재료학회 Metals and Materials International Metals and Materials International Vol.30 No.2
발행연도
2024.2
수록면
348 - 359 (12page)
DOI
10.1007/s12540-023-01520-9

이용수

표지
📌
연구주제
📖
연구배경
🔬
연구방법
🏆
연구결과
AI에게 요청하기
추천
검색

초록· 키워드

오류제보하기
Ultra-low carbon (ULC) steels, containing a carbon content ~ 0.055 wt%, have been used in several applications in the formof thin foils. However, there are limited studies on the effects of foil thickness (t) to grain size (d) ratio and foil condition onthe tensile response and formability of thin ULC steel foils. In the present work, the tensile and forming behaviours of ULCsteel foils of thickness about 400 μm were evaluated in both annealed and prestrained (by cold reduction to 2–7%) conditionsas a function of t/d ratio and followed by detailed texture evolution analysis. Vacuum annealing was used to achievevarying t/d ratios in the specimens. Additionally, thin ULC steel foils of 100 μm thickness in annealed condition were alsoused for examining the thickness effect. Microstructural analysis was performed using the electron backscattered diffractiontechnique. Microformability was assessed by a miniaturised Nakazima test setup with specimen geometries designed toproduce three different strain paths. The annealed foils displayed a typical yield-point phenomenon, but the total yield-pointelongation decreased with decreasing thickness and grain size. The foils exhibited typical Hall–Petch strengthening, coldwork hardening, and forming limit curves; however, there were substantial reductions in both tensile strength and ductility,and consequently, the forming strains, with decreasing the t/d ratio. The tensile response and formability of the foils wereadversely affected by both thinning and prestraining. The texture studies revealed the formation of a γ-fibre i.e., < 111 >||normaldirection, and its intensity varied significantly with the t/d ratio and mode of strain path.