메뉴 건너뛰기
.. 내서재 .. 알림
소속 기관/학교 인증
인증하면 논문, 학술자료 등을  무료로 열람할 수 있어요.
한국대학교, 누리자동차, 시립도서관 등 나의 기관을 확인해보세요
(국내 대학 90% 이상 구독 중)
로그인 회원가입 고객센터 ENG
주제분류

추천
검색

논문 기본 정보

자료유형
학술저널
저자정보
Maulana, Sena (Department of Forest Products, Faculty of Forestry, Bogor Agricultural University, IPB Dramaga Campus) Gumelar, Yuarsa (Department of Forest Products, Faculty of Forestry, Bogor Agricultural University, IPB Dramaga Campus) Fatrawana, Adesna (Forestry Study Program, Faculty of Agriculture, Khairun University) Maulana, Muhammad Iqbal (Department of Forest Products, Faculty of Forestry, Bogor Agricultural University, IPB Dramaga Campus) Hidayat, Wahyu (Department of Forestry, Faculty of Agriculture, Lampung University) Sumardi, Ihak (School of Life Sciences and Technology, Bandung Institute of Technology) Wistara, Nyoman Jaya (Department of Forest Products, Faculty of Forestry, Bogor Agricultural University, IPB Dramaga Campus) Lee, Seung Hwan (Department of Forest Biomaterials Engineering, College of Forest and Environmental Science, Kangwon National University) Kim, Nam Hun (Department of Forest Biomaterials Engineering, College of Forest and Environmental Science, Kangwon National University) Febrianto, Fauzi (Department of Forest Products, Faculty of Forestry, Bogor Agricultural University, IPB Dramaga Campus)
저널정보
한국목재공학회 목재공학(Journal of the Korean Wood Science and Technology) 목재공학 제47권 제4호
발행연도
2019.1
수록면
519 - 532 (14page)

이용수

표지
📌
연구주제
📖
연구배경
🔬
연구방법
🏆
연구결과
AI에게 요청하기
추천
검색

초록· 키워드

오류제보하기
The objectives of this study were to evaluate the effects of shelling ratio and resin content on the properties of bamboo oriented strand board (BOSB) from betung (Dendrocalamus asper) and to determine the correlation between the results of dynamic and static bending tests. Strands were steam-treated at $126^{\circ}C$ for 1 h under 0.14 MPa pressure and followed by washing with 1% NaOH solution. Three-layer BOSB with the core layer perpendicular to the surface was formed with shelling ratios (face:core ratio) of 30:70; 40:60; 50:50; 60:40 and binded with 7% and 8% of phenol formaldehyde (PF) resin with the addition of 1% of wax. The evaluation of physical and mechanical properties of BOSB was conducted in accordance with the JIS A 5908:2003 standard and the results were compared with CSA 0437.0 standard for commercial OSB (Grade O-1). Non-destructive testing was conducted using Metriguard Model 239A Stress Wave Timer which has a wave propagation time from 1 to $9,999{\mu}s$ and a resolution of $1{\mu}s$. BOSB with 8% resin content showed better physical and mechanical properties than those with 7% resin content. The increase of the face layer ratio improved the strength of BOSB in parallel direction to the grain. The results suggested that shelling ratio of 50:50 could be used as a simple way to reduce PF resin requirements from 8% to 7% and to meet the requirements of CSA 0437.0 standard. The results of non-destructive and destructive tests showed a strong correlation, suggesting that non-destructive test can be used to estimate the bending properties of BOSB.