In this study for evaluating properties of concrete according to extra-water quantitatively, compressive strength which is a clause of concrete quality control and shrinkage which is able to measure in the same time were compared.
As a result, extra-water limit of concrete unit-water content can be presumed +20㎏/㎥ through the compressive strength for concrete quality control. Considering that revelation ratio of compressive strength were similar each age, if it can be known compressive strength of plain specimen, it is able to presume unit-water content and extra-water of concrete in early age. And limit of dry shrinkage appeared 9.2~9.3×10-6/day, limit ratio of shrinkage by plat-ring restrained test appeared 1.5~1.7 ratio. Limit of cracking dimensions and cracking point appeared 100㎡ and 25point.

목차

Abstract
1. 서론
2. 실험계획
3. 실험결과 및 고찰
3. 결론
참고문헌

참고문헌 (0)

참고문헌 신청

함께 읽어보면 좋을 논문

논문 유사도에 따라 DBpia 가 추천하는 논문입니다. 함께 보면 좋을 연관 논문을 확인해보세요!

이 논문의 저자 정보

이 논문과 함께 이용한 논문

최근 본 자료

전체보기

댓글(0)

0

UCI(KEPA) : I410-ECN-0101-2010-540-001657423